According to product groups due to various reasons this problem occurs.
a) If synthetic, shiny or old painted surfaces yarımat and if a painting is done; emery emery powder made from the environment as long as this problem occurs is not clear. Adhesion performance of paint to a bright surface is low, it should be carried out sandpaper and emery powder should be removed from the environment.
b) If the new will be painted, the surface with putty or gypseous; ilkastarın and dust on the surface of araastarın enough to continue and not do, however, is the main cause adhesion problems. This type of problem in general practice in the form of breaking away from the plaster itself indicates.
Troubleshooting Methods: Surface preparation is required to, if the glass surface or lining gypseous process is done, according to information lejant painting process is done again.