..: Epoxy Repair Methods for Pre-Application :..
Crack types
• shrivel up in the cracks:
Required in concrete "tensile strength" is reached that the water vapor created cracks, 0,1 - 0,2 mm in width and consists Pentapox S / L can be repaired by using the primer.
• Temperature Difference of Crack:
During the curing of concrete is exposed to different temperatures, can cause cracks to. The crack widths at the time of curing according to the temperature change is different in size. Such cracks are not necessarily V-shaped break genişletilerek, should be restored by L Pentapox Epoxy Grout.
• Cold joints are (Construction of joints)
Concrete cast in place ano combination of "cold joints" are formed. This epoxy coating is applied on joints and cracks after a while the inevitable. Epoxy coating to prevent cracks in the cracks that will occur, V-shaped extend, Pentapox Grut L 30 can be filled, and can be reinforced with glass fibers, by using the Clear Coat Pentapox laminated edilmeli.Crack Bridging Materials
Will not be applied to the surface degradation of epoxy in combination ano / break are being used to prevent progress. Ano combination cracks in places, especially from forklift traffic to avoid damage to be done are used in repair, due to elastic structures ger be able to receive elastomeric joints, but according to the filling is very hard due to the structure of mechanical strength is high, this type of material required, the "elongation at break" can be produced in hardness.
Repair of joints Dilatasyon
Epoxy coating on the surface, needs to focus on one of the most important details of the existing floor joints in dilatasyon. Applying the appropriate solution of epoxy coated joints are dilatasyon over time, the crack on the epoxy coating causes the coating should have the repairs.
For this reason, before being passed to the coating on both sides of joints 7-8 cm wide and 7-8 cm depth with the machine is breaking Hilti breakers. All dirt and concrete as the weak parts will be cleaned by sweeping out and received. The resulting kaviteye (30.30.3) korniyer and both sides are placed Pentapox Epoxygrout the space L30 (750 kg / cm ²) with the pressure resistance is filled with epoxy repair fee.
Joints in space "backup cord" is placed after the above "sealent" and get off the ground is suitable for coating by.
Protection of concrete floor and container on the most appropriate solutions to needs in producing the EPONE, find solutions to problems applications.
|